This is the full data set from the UTEC Tissue testing lab on 10/18/2019 -unconfined compression test of cartilage sample -5 mm diameter Thickness = 1.44 mm Tests: 1. Sample is compressed to 15% strain at 5%/s, 10%/s and 15%/s strain rate. 2. Cyclic loading for pre-conditioning: 100 cycles between 10% and 15 % strain are applied at 2Hz. 3. Stress relaxation: Sample is compressed to 15% strain at 20%/s and held for 4 minutes.